Cracks and prevention of malleable steel pipe castings

Feb 20, 2023

info-790-732

 

When the casting internal stress exceeds the strength limit of the metal, the casting will produce cracks. Cracks can be divided into hot cracks and cold cracks.

 

(1) hot crack
Hot tearing is a crack produced by castings at high temperature, and it is one of the most common casting defects in the production of steel castings, malleable cast iron blanks and some light alloy castings. Its characteristics are: the appearance of the crack is tortuous and irregular, the surface of the crack is oxidized (the crack surface of the steel casting is approximately black, while the aluminum alloy is dark gray), and there is no metallic luster; the crack passes along the grain boundary. Hot cracks are generally distributed in the parts that are prone to stress concentration in the casting or inside the final solidification part of the casting.

 

(2) Cold cracking
Cold cracks are cracks that occur in castings at low temperatures. Alloys with poor plasticity, high brittleness, and low thermal conductivity, such as white cast iron, high carbon steel, and some alloy steels, are most prone to cold cracks. Its characteristics are: the shape is continuous and linear (no branch) or smooth curve, the surface of the crack is clean, with metallic luster, and sometimes a slight oxidation color. Cold cracks often appear on the surface of castings and often break through grains rather than along grain boundaries.

Cracks are serious defects of castings, which often make castings scrapped, so we must try to prevent them. In terms of design, the casting structure should be reasonably designed to reduce the internal stress of the casting; in terms of technology, the content of phosphorus and sulfur should be reduced, and the yield of the mold (core) sand should be improved and the time for opening the box should be controlled.