What elements are contained in Jianzhi malleable steel pipe fittings?

Jun 09, 2023

With the rapid development of my country's economy, the demand for malleable iron pipe fittings (commonly known as malleable steel pipe fittings) for water, gas and oil passages is increasing day by day, and the requirements for its quality are also getting higher and higher.

The applicability of Jianzhi malleable steel pipe fittings to the size of castings, castings produced by negative pressure compact casting, unlike magnetic casting, are limited by the size of the magnetic pole spacing. As long as the size of the magnetic pole is fixed, the size of the sand box is also fixed. It is almost impossible to cast a casting that exceeds the size of the sand box, which is generally only suitable for pouring small pieces of one hundred and ten kilograms. Negative pressure solid indium casting is much more applicable to the size of castings. Sand boxes of different sizes can be placed on the same vibration table, so castings of various sizes can be produced very conveniently.

However, due to the low strength of the foam plastic model and the fact that the filling cannot be absolutely uniform during the embedding operation, the model is easily deformed, which brings certain difficulties to casting large, narrow and thin castings. Therefore, considering the convenience of operation and the existing technology level, it is advisable to cast castings with a negative pressure compact casting of less than 2t (especially 500kg) and a wall thickness greater than 4mm.

The direct cause of mold sticking caused by Jianzhi malleable steel is that the strength of the molding sand is too low, that is, the adhesion force between sand grains is less than the adhesion force of sand grains on the pattern. The specific reasons are as follows:

1. Casting and pattern design

(1) Due to improper design, the draft angle is not enough. If the draft angle of the pattern is too small, it will form an adsorption effect, which will increase the friction force and lead to the loosening of the surface of the molding sand.

(2) The casting design contains deep and narrow depressions. The hanging sand in this concave part is easy to break when the mold is lifted. In this case, use sand hooks and sand-fixing wood chips to strengthen the sand in this part.

2. Appearance

(1) The surface of the pattern is not smooth or the coating is rough. This can result in sand particles adhering to the surface of the pattern in scattered or clumped patterns. When sanding, because the surface of the pattern is rough, the molding sand will be pounded into the depression on the surface of the pattern, and this part of the sand will loosen or fall off when the mold is removed.

(2) The coating used for the pattern is improper, and it is easy to adhere to the sand grains.

(3) There are pits or looseness at the parting surface. In this way, when the mold is removed, the molding sand sticks to the pattern.

3. Sand box and its preparation

(1) The rigidity of the sand box is too poor. During extrusion molding, the rigidity of the sand box is too poor, which will cause the sand box to rebound or deform. When the pressure is released, if the sand box rebounds, it will squeeze the concave part of the sand mold. The molding sand will stick to the pattern, thus forming succulents.

(2) The height of the sand box is not enough. Because the height of the sand box is not enough, the hanging sand may be too tight, so the friction force is very large when the mold is opened, resulting in loose hanging sand.

(3) If there are too many patterns placed in a sand box of a certain size, it is easy to cause uneven spring sand and uneven compactness, thus making the molding sand brittle.

(4) Excessive vibration of the pattern causes the hanging sand to break under the action of shear force.