The production points of elbow
Mar 12, 2022
1. The electrode should be kept dry during use. The titanium calcium type should be dried at 150 °C for 1 hour, and the low hydrogen type should be dried at 200-250 °C for 1 hour (do not repeat drying for many times, otherwise the coating will be easy to crack and peel off) to prevent the electrode The coating sticks to oil and other dirt, so as not to increase the carbon content of the weld and affect the quality of the weldment. When the elbow is welded, it is repeatedly heated to precipitate carbides, which reduce the corrosion resistance and mechanical properties. After welding, the hardenability is large, and cracks are prone to occur. If the same type of electrode is used for welding, it must be preheated above 300 °C and slowly cooled at about 700 °C after welding. If the weldment cannot be subjected to post-weld heat treatment, a chrome-nickel stainless steel electrode should be used.
2. In order to improve the corrosion resistance and weldability of stainless steel elbows, appropriate amount of stable elements such as Ti, Nb, Mo, etc. are appropriately added, and the weldability is better. When using the same type of chromium stainless steel electrode, it should be preheated above 200 ℃ And tempering treatment at about 800 ℃ after welding. If the weldment cannot be heat treated, a chrome-nickel stainless steel electrode should be used.