The preparation process of water-based paint is roughly as follows:
First add refractory material, bentonite, anhydrous sodium carbonate and other dry materials into the sand mixer, dry mix left and right - add binder solution and a little water, wet mix for about 20-30min - + wet material is rolled out Pour it into a mixing bucket, add an appropriate amount of water and stir, and add other additives during the stirring.

From the technical point of view, the speed of the agitator is required to be greater than 1380r/min, and the stirring time is greater than 1h. Production practice has proved that the rotation speed and stirring time of the agitator affect the coating performance and precipitation of the paint. The speed of the agitator is high, the stirring time is long, the paint is mixed more evenly, it is not easy to settle, and the coating effect is good.

The ball mill is used to prepare the paint. Due to the ball milling effect, the paint can be fully mixed to reach a colloidal state, and the coating effect is better. The preparation process is as follows: add refractory material, activated bentonite and a little water into the ball mill, ball mill for 7-8 hours-add the prepared binder aqueous solution, then ball mill, pour the paint into the paint bucket or use compressed air to press it into the paint bucket to fully Stir (the operation is the same as above), and add some additives depending on the air permeability of the paint.